High Tensile Strength Platinum Cured Silicone Rubber
This product has been discontinued and removed from our shelves.
Inquiry
Applications
This platinum cured silicone rubber is featured by high tensile strength, suitable for manufacturing sheaths, wallets, watchbands, elastic bands, jewelries and other various products whose tensile strength is highly required.
Features
- Rapid vulcanization;
- Non-yellowing;
- Easy de-molding;
- High tensile strength and tear strength;
- Similar performance to fumed silicone rubber;
- Suitable for manual edge finishing;
Approvals
ROHS, REACH, FDA, CA65, EN71-3, EN14372, PAHS, PFOA, CPSIA, siloxane testing, etc.
Test
Addition A type agent 0.5%, B type agent 0.8%, 120℃×3min×15Mpa
Technical Data
- Model: HT-8130A
- Appearance: Translucent
- Processability: 200-200
- Hardness (Shore A): 30
- Density (g/cm3): 1.12
- Tensile strength (Mpa): 6
- Elongation (%): 850
- Tear strength (K N/m): 20
- Model: HT-8140A
- Appearance: Translucent
- Processability: 220-240
- Hardness (Shore A): 40
- Density (g/cm3): 1.13
- Tensile strength (Mpa): 7
- Elongation (%): 750
- Tear strength (K N/m): 40
- Model: HT-8150A
- Appearance: Translucent
- Processability: 220-240
- Hardness (Shore A): 50
- Density (g/cm3): 1.14
- Tensile strength (Mpa): 8
- Elongation (%): 650
- Tear strength (K N/m): 50
- Model: HT-8160A
- Appearance: Translucent
- Processability: 230-260
- Hardness (Shore A): 60
- Density (g/cm3): 1.15
- Tensile strength (Mpa): 8
- Elongation (%): 550
- Tear strength (K N/m): 50
- Model: HT-8170A
- Appearance: Translucent
- Processability: 260-280
- Hardness (Shore A): 70
- Density (g/cm3): 1.2
- Tensile strength (Mpa): 9
- Elongation (%): 450
- Tear strength (K N/m): 50
- Model: HT-8180A
- Appearance: Translucent
- Processability: 250-280
- Hardness (Shore A): 80
- Density (g/cm3): 1.2
- Tensile strength (Mpa): 8
- Elongation (%): 300
- Tear strength (K N/m): 40
- Model: HT-8190A
- Appearance: Translucent
- Processability: 260-290
- Hardness (Shore A): 90
- Density (g/cm3): 1.22
- Tensile strength (Mpa): 6
- Elongation (%): 200
- Tear strength (K N/m): 40